FALL SAVINGS! TAKE 40% OFF YOUR NEXT ORDER, UP TO $400. USE CODE FALL40.

Atomic Layer Deposition Overview

Megan Conniff
Written byMegan Conniff
24 min read
Published September 30, 2026

Atomic layer deposition is a thin-film deposition technique that builds material coatings one atomic monolayer at a time through sequential, self-limiting surface chemical reactions. Atomic layer deposition occupies a foundational role in nanoscale precision manufacturing, where controlling film thickness at the sub-nanometer level determines the electrical, chemical, and structural performance of the finished component.

The technique's relevance to semiconductor fabrication stems from its capacity to deposit gate dielectrics, diffusion barriers, and capacitor liners with thickness uniformity below 1% across complex three-dimensional structures that conventional deposition methods cannot coat conformally. Industrial adoption of atomic layer deposition extends from logic and memory chip production to medical device coatings, flexible packaging barriers, and corrosion-resistant surface treatments. Node generations at 7 nm, 5 nm, and 3 nm depend on atomic layer deposition for gate oxide layers where a deviation of a single atomic plane alters transistor leakage and switching performance. Production systems operate at substrate temperatures from 25°C to 400°C, accommodating temperature-sensitive materials including polymers, biological surfaces, and pre-processed semiconductor wafers. The global atomic layer deposition equipment market reflects the technique's industrial centrality, with installed capacity expanding across logic, DRAM, NAND flash, and advanced packaging manufacturing facilities worldwide.

What Is Atomic Layer Deposition?

Atomic layer deposition is a vapor-phase thin-film deposition process that grows conformal material coatings on a substrate surface through alternating, self-limiting chemical reactions between gaseous precursor molecules and the substrate surface. Each deposition cycle introduces one precursor gas into the reaction chamber, allowing it to chemisorb onto available surface sites until the reaction terminates by saturation. A purge step removes excess precursor and reaction byproducts, followed by exposure to a second reactant that converts the chemisorbed layer into the target film material. The four-step sequence (precursor dose, purge, co-reactant dose, purge) constitutes one ALD cycle and deposits a defined sub-monolayer to monolayer increment of the target material, typically from 0.5 Å to 3 Å per cycle.

The self-limiting nature of each half-reaction prevents precursor accumulation beyond one molecular layer per cycle, establishing the process's defining characteristic of atomic-scale thickness control. Film thickness is set by the number of completed cycles rather than by deposition time, gas flux, or substrate position in the chamber. The mechanism produces conformal coatings on surfaces with aspect ratios from 10:1 to above 1000:1, coating the floors, walls, and ceilings of deep trench structures and high-aspect-ratio nanopores with the same film thickness as flat reference surfaces on the same substrate.

What Is Atomic Layer Deposition Equipment?

Atomic layer deposition equipment refers to precision deposition systems engineered to deliver alternating precursor and co-reactant gases to a substrate surface under controlled temperature and vacuum conditions, executing the sequential self-limiting reaction cycles that build conformal thin films one atomic layer at a time. The systems range from laboratory-scale single-wafer research tools processing 200 mm substrates to production-scale batch reactors handling 25 or more 300 mm wafers per load.

The core system components include the reaction chamber, precursor delivery and vapor management hardware, vacuum pumping and pressure control subsystems, a thermal management system for substrate and chamber temperature control, and a process control platform that sequences gas flows, timing, temperature, and purge intervals across each deposition cycle. Plasma-enhanced ALD (PE-ALD) systems incorporate an additional radio-frequency plasma source that activates the co-reactant at lower substrate temperatures than thermally driven processes. Spatial ALD systems replace time-sequenced gas switching with substrate translation from zone to zone, enabling deposition rates from 10 to 100 nm per minute compared to 0.1 to 2 nm per minute on conventional time-domain systems. Equipment configuration determines the substrate size, throughput, film material range, and minimum achievable deposition temperature for a given production application.

Which Components Make Up ALD Equipment?

The components that make up ALD equipment are listed below. 

  • Reaction Chamber: The reaction chamber is a sealed enclosure constructed from stainless steel, aluminum, or quartz that confines the substrate and the alternating precursor gases during each deposition cycle. Chamber geometry determines gas flow distribution across the substrate surface, with cross-flow, showerhead, and rotary designs each producing different uniformity profiles. Chamber wall temperature is actively controlled from 60°C to 150°C to prevent precursor condensation on internal surfaces that would contaminate the deposition environment.
  • Precursor Delivery System: The precursor delivery subsystem stores liquid or solid precursor materials in temperature-controlled vessels called bubblers or ampoules and delivers controlled vapor doses to the reaction chamber through heated gas lines and automated pneumatic valves. Precursor vessel temperature determines vapor pressure and dose rate, with common precursors operating at vessel temperatures from 20°C to 120°C. Valve switching times from 10 ms to 100 ms define the dose pulse duration and determine cycle time at the millisecond scale.
  • Vacuum System: The vacuum pumping system maintains chamber operating pressures from 0.01 Torr to 10 Torr during deposition, depending on the process chemistry and reactor design. Dry mechanical pumps and turbomolecular pumps are selected based on precursor chemistry compatibility, with corrosive process chemistries requiring chemically resistant pump materials. Pressure control valves and capacitance manometers maintain chamber pressure within ±1% of the setpoint during each precursor and purge step.
  • Thermal Management System: Resistive heating elements, thermocouples, and PID temperature controllers maintain the substrate chuck temperature within ±0.5°C of the target process temperature across the full substrate area. Substrate temperatures from 25°C (plasma-enhanced processes) to 400°C (thermal processes) are achievable depending on the reactor and precursor chemistry. Chamber wall temperature control prevents precursor condensation and limits parasitic CVD-mode deposition on internal surfaces.
  • Process Control Platform: The PLC or dedicated software control platform sequences precursor valve actuation, purge gas flow, plasma ignition timing, pressure setpoints, and temperature profiles across each ALD cycle with millisecond timing precision. Recipe storage systems allow recall of validated process parameters for production repeatability across hundreds of thousands of deposition cycles. Data logging functions record process parameters at each cycle for quality traceability and drift analysis in production environments.

What Role Does Atomic Layer Deposition (ALD) Play in Semiconductor Processing?

Atomic layer deposition serves as the deposition method of choice for gate dielectric layers, diffusion barrier films, capacitor dielectrics, and contact liner materials in advanced semiconductor fabrication, where film thickness from 1 nm to 10 nm must be controlled at the atomic level to meet transistor performance specifications. In gate stack fabrication, ALD deposits high-k dielectric materials (hafnium oxide, HfO₂, at thicknesses from 1 nm to 3 nm) that replace silicon dioxide as the gate insulator in logic transistors at 45 nm node and below. The equivalent oxide thickness (EOT) achievable with ALD-deposited HfO₂ falls from 0.5 nm to 1.5 nm, enabling continued gate capacitance scaling without the leakage current increase that thinner SiO₂ layers would produce.

Barrier layer deposition in copper interconnect systems relies on ALD to coat the sidewalls and floors of high-aspect-ratio via structures with tantalum nitride (TaN) or titanium nitride (TiN) films from 2 nm to 5 nm thick. The conformal coverage of ALD barrier layers prevents copper diffusion into the surrounding low-k dielectric at the sub-10 nm liner thicknesses that sputtered physical vapor deposition cannot achieve reliably on aspect ratios above 5:1. ALD also deposits the nucleation layers for electroplated copper fill, the capacitor dielectrics in DRAM storage cells, and the charge trap layers in 3D NAND flash memory stacks.

Why Is ALD Important for Advanced Semiconductor Nodes?

ALD is indispensable at advanced semiconductor nodes because transistor gate lengths below 10 nm require gate dielectric films with thickness uniformity measured in fractions of an atomic layer, a level of control that no alternative deposition method achieves across full 300 mm wafer areas. At the 5 nm and 3 nm nodes, the gate oxide layer must maintain a physical thickness from 1 nm to 2 nm while delivering an EOT from 0.4 nm to 0.8 nm with leakage current density below 10⁻² A/cm². Thickness variation above 0.1 nm across the wafer introduces statistical spread in transistor threshold voltage that widens timing margins and degrades circuit performance.

Leakage current reduction at advanced nodes depends directly on ALD's ability to deposit pinhole-free dielectric films with interface state densities below 10¹¹ cm⁻² eV⁻¹ at the high-k/silicon interface. Pinholes or interface defects in the gate dielectric provide direct current paths from gate to channel, increasing standby power consumption and reducing device reliability. ALD's self-limiting reaction mechanism deposits material only where surface hydroxyl groups are present, eliminating the film discontinuities that appear in CVD and PVD films at sub-2 nm thicknesses. Performance improvement at each successive node generation depends on ALD maintaining dielectric integrity at thicknesses approaching the fundamental limits of the material system.

How Does Atomic Layer Deposition Support Scaling Challenges in Advanced Semiconductor Technologies?

Atomic layer deposition supports semiconductor scaling by providing atomic-level thickness control, conformal coverage on high-aspect-ratio structures, and precise material sequencing that no competing thin-film deposition technique delivers simultaneously at production scale. At each successive node generation, the geometric features of transistors, capacitors, and interconnect structures shrink while their aspect ratios increase, creating deposition environments where film conformality and thickness uniformity become the primary process constraints rather than deposition rate.

Thickness control at the sub-angstrom level per cycle allows ALD to define the gate dielectric, barrier, and capacitor films with a precision that scales with cycle count rather than with analog process variables like time or pressure. Conformal coating of structures with aspect ratios from 50:1 to above 100:1 in 3D NAND flash memory stacks is achievable with ALD because the self-limiting reaction mechanism deposits equivalent thickness on all exposed surfaces regardless of their depth below the wafer top surface. Precise material layering in nanolaminates (alternating HfO₂/Al₂O₃ stacks, for example) allows dielectric constant and band offset engineering at the atomic scale, expanding the material design space available to device engineers. The combination of thickness control, conformality, and material flexibility makes atomic layer deposition the enabling deposition technology for continued transistor and memory cell scaling below 5 nm feature dimensions.

How Is ALD Applied in Chip Fabrication Steps?

ALD is applied in chip fabrication steps by following the five steps listed below. 

  1. Gate Dielectric Deposition: The silicon substrate surface is prepared with a thermal or chemical oxide passivation treatment to establish a controlled interface before ALD. The high-k dielectric layer (HfO₂ or HfSiON) is deposited by ALD at substrate temperatures from 250°C to 350°C to a physical thickness of 1 nm to 3 nm, defining the transistor gate capacitance.
  2. Metal Gate Liner Deposition: The ALD deposits a metal nitride work-function layer (TiN, TaN, or TiAlC) directly on the high-k dielectric surface to set the transistor threshold voltage for NMOS or PMOS device types. The metal gate liner thickness from 2 nm to 5 nm is controlled by cycle count, with process temperature from 300°C to 400°C.
  3. Barrier Layer Deposition in Interconnects: Following via and trench etching in the dielectric stack, ALD deposits a conformal TaN or TiN diffusion barrier from 2 nm to 4 nm thick on all via and trench surfaces before copper electroplating fill. The barrier prevents copper diffusion into the surrounding low-k dielectric at thicknesses that sputtered PVD cannot achieve conformally on aspect ratios above 5:1.
  4. Capacitor Dielectric Deposition in DRAM: The ALD deposits the capacitor dielectric (ZrO₂/Al₂O₃ nanolaminates) inside high-aspect-ratio capacitor cylinder structures with aspect ratios from 50:1 to 80:1 in DRAM storage cells. A film thickness from 5 nm to 10 nm is deposited conformally across the full cylinder depth to meet the capacitance and leakage specifications of the storage cell.
  5. Charge Trap Layer in 3D NAND: The ALD deposits the charge trap dielectric stack (SiO₂/Si₃N₄/SiO₂, or ONO) inside the memory hole structures of 3D NAND flash, where aspect ratios from 60:1 to over 100:1 require conformal deposition uniformity that no alternative process achieves at production yield. The ALD-deposited charge trap layer determines data retention time and program/erase cycling endurance of the finished memory cell.

Does ALD Improve Semiconductor Device Reliability?

Yes, ALD improves semiconductor device reliability by producing gate dielectric and barrier films with pinhole-free density, controlled interface chemistry, and thickness uniformity that reduce the primary failure mechanisms in advanced transistors and interconnect structures. Pinhole defects in gate dielectric films provide low-resistance current paths from the gate electrode to the transistor channel, accelerating time-dependent dielectric breakdown (TDDB) and reducing device operating lifetime below specification. ALD's self-limiting reaction mechanism eliminates pinholes by saturating every available surface site before the cycle advances, producing films with dielectric breakdown fields from 8 MV/cm to 12 MV/cm in HfO₂ layers deposited at standard process conditions.

Barrier layer reliability in copper interconnects depends on the ALD film covering via sidewalls and bottom corners without the thinning or voids that physical vapor deposition produces in high-aspect-ratio geometries at sub-5 nm thicknesses. Copper diffusion through a defective barrier creates conductive filaments in the surrounding dielectric, causing leakage and eventual dielectric breakdown at interconnect operating voltages. ALD TaN and TiN barriers with conformal coverage from 2 nm to 4 nm on aspect ratios above 10:1 provide copper diffusion resistance that extends mean time to failure in interconnect reliability testing from thousands to tens of thousands of hours at accelerated stress conditions.

Which Materials Are Associated With Atomic Layer Deposition in Industry?

Atomic layer deposition processes a defined range of substrate and precursor-derived materials. The ALD materials are used across the semiconductor, medical, aerospace, and packaging industries. The material is where atomic-scale film control determines the functional performance of the finished component or device. 

The materials associated with Atomic Layer Deposition in industry are listed below. 

  • Aluminum (Al): Aluminum substrates accept ALD-grown aluminum oxide (Al₂O₃) films through reaction with trimethylaluminum (TMA) precursor at deposition temperatures from 25°C to 300°C. The Al₂O₃ film provides electrical insulation with a dielectric constant from 7 to 9 and a breakdown field above 8 MV/cm, making it a standard passivation layer for power semiconductor devices and microelectromechanical systems. Hardness values from 10 GPa to 14 GPa in ALD Al₂O₃ coatings extend the service life of components in sliding contact and abrasive environments. The base element in ALD-deposited aluminum nitride (AlN) films for thermal management layers in high-power electronics packages is Aluminum (Al).
  • Copper (Cu): Copper interconnects in advanced logic and memory devices require ALD-deposited diffusion barrier layers that prevent copper atoms from migrating into surrounding low-k dielectric under thermal and electrical stress. ALD TaN and TiN barrier films from 2 nm to 4 nm thick coat via sidewalls and floors with aspect ratios from 5:1 to above 20:1, providing conformal coverage that sputtered physical vapor deposition cannot achieve at sub-5 nm thicknesses. Barrier integrity of ALD films limits copper diffusion to below 10¹⁵ atoms/cm² after 1,000 hours at 200°C, meeting reliability requirements of 7 nm and 5 nm node interconnect stacks. ALD nucleation seed layers that improve adhesion and void-free fill quality of electroplated Copper (Cu) in narrow interconnect trenches are a standard integration step at advanced nodes.
  • Silicon (Si): Silicon wafer surfaces receive ALD-deposited high-k gate dielectric films at the transistor gate stack position, where the ALD layer replaces thermally grown SiO₂ at nodes below 45 nm. ALD deposits HfO₂ at physical thicknesses from 1 nm to 3 nm directly on hydrogen-terminated or chemically oxidized silicon surfaces, achieving interface state densities below 5 × 10¹⁰ cm⁻² eV⁻¹ with optimized surface preparation protocols. The high dielectric constant of HfO₂, from 18 to 25, allows gate capacitance equivalent to 0.5 nm SiO₂ at a physical thickness that suppresses direct tunneling leakage by three to four orders of magnitude. ALD silicon nitride and silicon oxide films deposited on Silicon (Si) serve as spacer dielectrics, etch stop layers, and passivation films at multiple stages in the transistor fabrication sequence.
  • Titanium (Ti): Titanium substrates receive ALD-deposited titanium oxide (TiO₂) and titanium nitride (TiN) films for applications requiring photocatalytic activity, biocompatibility, or diffusion barrier performance. ALD TiO₂ on titanium implant surfaces produces a controlled anatase or rutile phase film from 5 nm to 50 nm thick that promotes osseointegration and resists corrosion from bodily fluids with a corrosion current density below 10⁻⁸ A/cm². ALD TiN on titanium aerospace components provides a hard surface layer with hardness from 22 GPa to 30 GPa that reduces wear and oxidation at service temperatures up to 500°C. The dimensional precision of ALD deposition preserves the tight tolerances of finished Titanium (Ti) components, adding functional surface properties without requiring regrinding or dimensional correction after coating.
  • Polyethylene Terephthalate (PET): PET films used in flexible food packaging and electronic display substrates accept ALD-deposited moisture and oxygen barrier layers at deposition temperatures from 25°C to 100°C, below the PET glass transition temperature of approximately 75°C to 80°C. ALD Al₂O₃ films from 10 nm to 30 nm thick on PET substrates reduce water vapor transmission rates from the uncoated value of approximately 10 g/m²/day to below 10⁻³ g/m²/day, meeting barrier requirements for flexible OLED display encapsulation. The conformal coating covers surface defects and micro-scratches in the PET film that serve as permeation pathways for moisture and oxygen in conventional thin-film barrier coatings. Polyethylene Terephthalate (PET) packaging films with ALD barrier layers extend the shelf life of oxygen-sensitive food products by factors of 5 to 20 compared to uncoated film.

1. Aluminum (Al)

Aluminum substrates and aluminum-containing surfaces accept ALD-grown aluminum oxide (Al₂O₃) films through reaction with trimethylaluminum (TMA) precursor at deposition temperatures from 25°C to 300°C. The Al₂O₃ film provides electrical insulation with a dielectric constant from 7 to 9 and a breakdown field above 8 MV/cm, making it a standard passivation layer for power semiconductor devices and microelectromechanical systems. The wear resistance of ALD Al₂O₃ coatings, with hardness values from 10 GPa to 14 GPa, extends the service life of aluminum components in sliding contact and abrasive environments. Aluminum (Al) is also the base element in ALD-deposited aluminum nitride (AlN) films used for thermal management layers in high-power electronics packages. 

2. Copper (Cu)

Copper interconnects in advanced logic and memory devices require ALD-deposited diffusion barrier layers that prevent copper atoms from migrating into the surrounding low-k dielectric under thermal and electrical stress. ALD TaN and TiN barrier films from 2 nm to 4 nm thick coat the sidewalls and floors of copper via structures with aspect ratios from 5:1 to above 20:1, providing conformal coverage that sputtered physical vapor deposition cannot achieve at sub-5 nm thicknesses. The barrier integrity of ALD films limits copper diffusion to below 10¹⁵ atoms/cm² after 1,000 hours at 200°C, meeting the reliability requirements of 7 nm and 5 nm node interconnect stacks. ALD also deposits copper nucleation seed layers that improve the adhesion and void-free fill quality of electroplated Copper (Cu) in narrow interconnect trenches. 

3. Silicon (Si)

Silicon wafer surfaces receive ALD-deposited high-k gate dielectric films at the transistor gate stack position, where the ALD layer replaces thermally grown SiO₂ at nodes below 45 nm. ALD deposits HfO₂ at physical thicknesses from 1 nm to 3 nm directly on hydrogen-terminated or chemically oxidized silicon surfaces, achieving interface state densities below 5 × 10¹⁰ cm⁻² eV⁻¹ with optimized surface preparation protocols. The high dielectric constant of HfO₂ (from 18 to 25) allows gate capacitance equivalent to 0.5 nm SiO₂ at a physical thickness that suppresses direct tunneling leakage by three to four orders of magnitude. ALD silicon nitride and silicon oxide films deposited on Silicon (Si) also serve as spacer dielectrics, etch stop layers, and passivation films at multiple stages in the transistor fabrication sequence. 

4. Titanium (Ti)

Titanium substrates receive ALD-deposited titanium oxide (TiO₂) and titanium nitride (TiN) films for applications requiring photocatalytic activity, biocompatibility, or diffusion barrier performance. ALD TiO₂ on titanium implant surfaces produces a controlled anatase or rutile phase film from 5 nm to 50 nm thick that promotes osseointegration and resists corrosion from bodily fluids with a corrosion current density below 10⁻⁸ A/cm². ALD TiN on titanium aerospace components provides a hard (22 GPa to 30 GPa), chemically resistant surface layer that reduces wear and oxidation at service temperatures up to 500°C. The dimensional precision of ALD deposition preserves the tight tolerances of finished Titanium (Ti) components, adding functional surface properties without requiring regrinding or dimensional correction after coating. 

5. Polyethylene Terephthalate (PET)

PET films used in flexible food packaging and electronic display substrates accept ALD-deposited moisture and oxygen barrier layers at deposition temperatures from 25°C to 100°C, below the PET glass transition temperature of approximately 75°C to 80°C. ALD Al₂O₃ films from 10 nm to 30 nm thick on PET substrates reduce water vapor transmission rates from the uncoated value of approximately 10 g/m²/day to below 10⁻³ g/m²/day, meeting the barrier requirements for flexible OLED display encapsulation. The conformal coating covers surface defects and micro-scratches in the PET film that serve as permeation pathways for moisture and oxygen in conventional thin-film barrier coatings. Polyethylene Terephthalate (PET) packaging films with ALD barrier layers extend the shelf life of oxygen-sensitive food products by factors from 5 to 20 compared to uncoated film. 

What Are the Industrial Applications of Atomic Layer Deposition?

Atomic layer deposition serves industrial manufacturing sectors where conformal, pinhole-free, atomically precise thin films. Atomic layer deposition determines the functional performance, reliability, and service life of finished components. ALD is used across semiconductor fabrication, surface protection, packaging, and medical device production.

The industrial applications of Atomic Layer Deposition are listed below. 

  • Semiconductor Barrier Layers: ALD deposits conformal diffusion barrier films (TaN, TiN, WN) inside high-aspect-ratio via and trench structures of copper and tungsten interconnect systems in logic and memory chips. The self-limiting reaction mechanism ensures equal film thickness on via sidewall, corner, and floor surfaces regardless of structure depth, with conformality above 95% on aspect ratios from 10:1 to 30:1. Barrier films from 2 nm to 5 nm thick block metal diffusion into surrounding low-k dielectric layers while consuming minimal via volume, preserving the cross-sectional area available for conductive metal fill. Semiconductor barrier layers at the 7 nm and 5 nm nodes represent a mandatory process step with no conformal alternative at the required thickness range.
  • Corrosion-resistant Coatings: ALD deposits dense, pinhole-free oxide and nitride barrier layers (Al₂O₃, TiO₂, ZrO₂) on metal, polymer, and ceramic substrates to block moisture, oxygen, and aggressive chemical species from reaching the base material. Film density in ALD-deposited Al₂O₃ reaches 3.0 g/cm³ to 3.5 g/cm³, approaching the theoretical density of bulk alumina and leaving no permeation pathways through the film at thicknesses above 10 nm. Corrosion current densities on ALD-coated stainless steel surfaces fall to below 10⁻⁹ A/cm² in 3.5% NaCl solution, compared to 10⁻⁶ A/cm² to 10⁻⁷ A/cm² for uncoated reference surfaces. ALD corrosion-resistant coatings from 20 nm to 100 nm thick protect aerospace fasteners, medical instrument surfaces, and precision optical components where thicker conventional coatings alter critical dimensions or optical performance.
  • Flexible Packaging Barriers: ALD deposits ultra-thin gas barrier films on flexible polymer substrates (PET, PEN, polyimide) at low temperatures from 25°C to 100°C, preserving substrate flexibility and preventing thermal deformation during the coating process. Al₂O₃ barrier layers from 10 nm to 50 nm thick reduce water vapor transmission rates on PET films from approximately 10 g/m²/day to below 10⁻³ g/m²/day, meeting encapsulation requirements for flexible OLED displays and sensitive electronic components. The ALD process coats existing surface defects and scratch channels in the polymer substrate that act as preferential moisture permeation paths in sputtered or evaporated barrier films. Flexible packaging barriers deposited by ALD extend shelf life for oxygen-sensitive food and pharmaceutical products by eliminating the pinhole permeation pathways that limit conventional polymer multilayer barrier films.
  • Medical Implant Coatings: ALD applies biocompatible ceramic coatings (Al₂O₃, TiO₂, ZrO₂, hydroxyapatite) on the surfaces of orthopedic implants, dental fixtures, cardiovascular stents, and neural electrodes at film thicknesses from 10 nm to 200 nm. The conformal deposition covers all surface features of complex implant geometries, including threaded surfaces, porous scaffolds, and microstructured areas designed to promote bone or tissue integration, without altering the dimensional tolerances of the finished device. TiO₂ and ZrO₂ ALD coatings on titanium and cobalt-chrome implant substrates reduce ion release rates by factors from 10 to 100 compared to uncoated surfaces, limiting exposure of surrounding tissue to metallic corrosion products. Medical implant coatings on porous bone scaffolds with pore diameters from 100 µm to 600 µm maintain full pore patency at the required coating thickness, preserving the open pore volume needed for vascularization and osseointegration.

1. Semiconductor Barrier Layers

ALD deposits conformal diffusion barrier films (TaN, TiN, WN) inside the high-aspect-ratio via and trench structures of copper and tungsten interconnect systems in logic and memory chips. The self-limiting reaction mechanism ensures equal film thickness on the via sidewall, corner, and floor surfaces regardless of structure depth, with conformality above 95% on aspect ratios from 10:1 to 30:1. Barrier films from 2 nm to 5 nm thick block metal diffusion into surrounding low-k dielectric layers while consuming minimal via volume, preserving the cross-sectional area available for conductive metal fill. ALD semiconductor barrier layers at the 7 nm and 5 nm nodes represent a mandatory process step with no conformal alternative at the required thickness range. 

2. Corrosion-Resistant Coatings

ALD deposits dense, pinhole-free oxide and nitride barrier layers (Al₂O₃, TiO₂, ZrO₂) on metal, polymer, and ceramic substrates to block moisture, oxygen, and aggressive chemical species from reaching the base material. Film density in ALD-deposited Al₂O₃ reaches 3.0 g/cm³ to 3.5 g/cm³, approaching the theoretical density of bulk alumina and leaving no permeation pathways through the film at thicknesses above 10 nm. Corrosion current densities on ALD-coated stainless steel surfaces fall to below 10⁻⁹ A/cm² in 3.5% NaCl solution, compared to 10⁻⁶ A/cm² to 10⁻⁷ A/cm² for uncoated reference surfaces. ALD corrosion-resistant coatings from 20 nm to 100 nm thick protect aerospace fasteners, medical instrument surfaces, and precision optical components where thicker conventional coatings would alter critical dimensions or optical performance. 

3. Flexible Packaging Barriers

ALD deposits ultra-thin gas barrier films on flexible polymer substrates (PET, PEN, polyimide) at low temperatures from 25°C to 100°C, preserving substrate flexibility and preventing thermal deformation during the coating process. Al₂O₃ barrier layers from 10 nm to 50 nm thick reduce water vapor transmission rates (WVTR) on PET films from approximately 10 g/m²/day to below 10⁻³ g/m²/day, meeting encapsulation requirements for flexible OLED displays and sensitive electronic components. The ALD process coats existing surface defects and scratch channels in the polymer substrate that act as preferential moisture permeation paths in sputtered or evaporated barrier films. Flexible packaging barriers deposited by ALD extend shelf life for oxygen-sensitive food and pharmaceutical products by eliminating the pinhole permeation pathways that limit conventional polymer multilayer barrier films. 

4. Medical Implant Coatings

ALD applies biocompatible ceramic coatings (Al₂O₃, TiO₂, ZrO₂, hydroxyapatite) on the surfaces of orthopedic implants, dental fixtures, cardiovascular stents, and neural electrodes at film thicknesses from 10 nm to 200 nm. The conformal deposition covers all surface features of complex implant geometries, including threaded surfaces, porous scaffolds, and microstructured areas designed to promote bone or tissue integration, without altering the dimensional tolerances of the finished device. TiO₂ and ZrO₂ ALD coatings on titanium and cobalt-chrome implant substrates reduce ion release rates by factors of 10 to 100 compared to uncoated surfaces, limiting the exposure of surrounding tissue to metallic corrosion products. ALD medical implant coatings on porous bone scaffolds with pore diameters from 100 µm to 600 µm maintain full pore patency at the required coating thickness, preserving the open pore volume needed for vascularization and osseointegration.

"When designing parts that require sub-nanometer coatings or deep, high-aspect-ratio features, designing for manufacturing means recognizing that geometry dictates gas flow. Understanding how precursor vapors saturate tight cavities and internal channels allows designers to select realistic tolerances and coating chemistries early, preventing costly prototype failures before committing to production tooling."

Audrius Zidonis headshotAudrius Zidonis PhDPrincipal Engineer at Zidonis Engineering

Does Atomic Layer Deposition Maintain Uniform Coating Thickness on Complex Surface Geometries?

Yes, atomic layer deposition maintains uniform coating thickness on complex surface geometries because the self-limiting reaction mechanism deposits material at every exposed surface site at an equal rate, independent of the site's position, orientation, or depth within the structure. The process relies on chemisorption saturation rather than flux directionality, meaning precursor molecules that enter deep into a trench, pore, or via structure react with available surface sites in exactly the same way as molecules contacting the flat top surface. Conformality values above 95% on structures with aspect ratios from 10:1 to over 100:1 are documented in production ALD processes for semiconductor and MEMS applications.

The uniformity advantage of ALD over physical vapor deposition (PVD) and chemical vapor deposition (CVD) becomes most significant on high-aspect-ratio features, curved surfaces, and re-entrant geometries where line-of-sight or diffusion-limited deposition methods produce film thinning at corners, sidewalls, and structure bottoms. PVD sputtering produces conformality below 20% on aspect ratios above 5:1, with severe thinning at via bottoms and corners. Thermal ALD maintains conformality above 98% on the same structures by allowing sufficient precursor exposure time for the diffusion front to saturate all available surface sites before the purge step removes excess reactant. Film thickness variation across a 300 mm wafer in production ALD systems falls within ±0.5% of the mean value at optimized process conditions.

Disclaimer

The content appearing on this webpage is for informational purposes only. Xometry makes no representation or warranty of any kind, be it expressed or implied, as to the accuracy, completeness, or validity of the information. Any performance parameters, geometric tolerances, specific design features, quality and types of materials, or processes should not be inferred to represent what will be delivered by third-party suppliers or manufacturers through Xometry’s network. Buyers seeking quotes for parts are responsible for defining the specific requirements for those parts. Please refer to our terms and conditions for more information.

Start Your Instant QuoteSTEP · STP · SLDPRT · STL · DXF · IPT · X_T · X_B · 3DXML · CATPART · PRT · SAT · 3MF · JTUpload Your Design
All uploads are secure and confidential
Megan ConniffMegan is the Content Director at XometryRead more articles by Megan Conniff

Get in Touch

Ready to start your next manufacturing project? Our team is here to help with quotes, technical questions, and custom solutions.

By entering your contact information, you are agreeing to receive email communications about Xometry products and services. You may update your subscriptions or unsubscribe from these communications at any time using the link at the bottom of every marketing email or by contacting support. For more information, review our Privacy Policy.